1. Precursors of polyimide, polyamic acid have been prepared successfully by reation of 4,4'-Oxydianiline(ODA) and 3,3',4,4'-Benzophenone tetracarboxylic dianhydride(BTDA). 2. The surface electrical resistance of the nanocomposites decreased from 1.28 × 10~(15) Ω/cm~2 (neat polyimide) to 2.82 × 10~8 Ω/cm~2 (5.0phr polyimide coated CNT/PI composites) 3. Volume resistance of the nanocomposites decreased from 1.53 × 10~(17) Ω-cm (neat polyimide) to 8.77 × 10~6Ω-cm (5.0phr polyimide coated CNT/PI composites).
机译:1.通过4,4'-羟二苯胺(ODA)和3,3',4,4'-苯甲酮四羧酸二酐(BTDA)的反应成功制备了聚酰亚胺,聚酰胺酸的前体。 2.纳米复合材料的表面电阻从1.28×10〜(15)Ω/ cm〜2(纯聚酰亚胺)降至2.82×10〜8Ω/ cm〜2(5.0phr聚酰亚胺涂层的CNT / PI复合材料)3。纳米复合材料的体积电阻从1.53×10〜(17)Ω-cm(纯聚酰亚胺)降至8.77×10〜6Ω-cm(5.0phr聚酰亚胺涂层的CNT / PI复合材料)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号