Characteristic features of heat treatment of aluminium-lithium alloys are connected mainlyrnwith a presence of the general hardening phase δ' (Al3Li) both independently and as arnshell on θ', θ", Al3Zr and Al3Sc phases of composite two-phase particles. Influence of thernmulti-step artificial ageing of Al-Li-Cu, Al-Li-Mg-Cu and Al-Li-Mg alloys on phaserncomposition, precipitates morphology (particle size and distance between them), presence and width of precipitated free zones along boundaries is studied. Usage of multi-step ageing regimes allows to increase a fracture toughness, corrosion resistance and thermal stability in comparison with one-step ageing for Al-Li alloys.
机译:铝-锂合金热处理的特征主要是与复合两相粒子的θ',θ”,Al3Zr和Al3Sc相分别独立地或以壳状存在一般硬化相δ'(Al3Li)的状态相联系。在相组成上对Al-Li-Cu,Al-Li-Mg-Cu和Al-Li-Mg合金进行多步人工时效,析出物形态(颗粒尺寸和它们之间的距离),沿边界析出的自由区的存在和宽度为与Al-Li合金的单步时效相比,多步时效制度的使用可以提高断裂韧性,耐腐蚀性和热稳定性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号