HYDROTHERMAL SULFIDATION OF CARBONATE-HOSTED ZINC-LEAD ORE WITH ELEMENTAL SULFUR

机译:元素硫对碳酸盐浸出的锌铅矿石的水热硫化

获取原文

摘要

Direct flotation of oxidized zinc-lead ore is characterized by recovery of zinc and lead only around 55% and 50%, respectively. Mineralogical analysis shows that the sample used in the present study is a carbonate hosted zinc-lead ore, with a zinc and lead carbonate content that accounts for 80.14% and 75.63% of the total minerals, respectively. The carbonate hosted zinc-lead ore was hydrothermally sulfidized with elemental sufur and the experimental data indicated that under the conditions employed up to 75% zinc and 82% lead sulfidation extent were achieved. As a result of pre-sulfidation followed by flotation, the recoveries of zinc and lead into flotation concentrate were over 90%. A flotation concentrate was obtained with 52% Zn and 37% Pb from the materials which was treated by sulfidation.
机译:氧化锌铅矿石的直接浮选的特征是锌和铅的回收率分别仅为55%和50%。矿物学分析表明,本研究中使用的样品是碳酸盐寄主的锌铅矿石,其中锌和碳酸铅的含量分别占总矿物质的80.14%和75.63%。用元素硫对碳酸盐承载的锌铅矿石进行水热硫化,实验数据表明,在所采用的条件下,锌的硫化率可达75%,铅的硫化程度达到82%。经过预硫化和浮选的结果是,浮选精矿中锌和铅的回收率超过90%。从经硫化处理的材料中获得浮选精矿,其中锌含量为52%,铅含量为37%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号