Using CaCl_2 as sintering aid, the Tb-doped (Ba_(0.859) Ca_(0.141)) (Zr_(0.106) Ti_(0.894)) O_3 (BCZT) ceramics were fabricated by conventional solid-state reaction method. The sintering temperature of ceramics decreases from about 1450°C down to about 1300°C. The SEM micrographs show that all ceramics sintered above 1300°C are very dense and have clear grain boundaries. A piezoelectric coefficient of d_(33) 659 pm/V was obtained at 0.3 mol.% Tb-doped (Ba_(0.859) Ca_(0.141)) (Zr_(0.106) Ti_(0.894)) O_3 with CaCl_2 sintered at 1350°C and residual polarization of that can reach 11.70 μC/cm~2. The results indicated that the excellent piezoelectric property could be a promising candidate for electronic industry purposes.
机译:使用CaCl_2作为烧结助剂,通过常规固态反应方法制造Tb掺杂(Ba_(0.859)Ca_(0.141))(Zr_(0.141))O_3(BCZT)陶瓷。 陶瓷的烧结温度从约1450℃降低至约1300℃。 SEM显微照片表明,所有烧结以上的陶瓷都非常密集,具有清晰的晶界。 在0.3摩尔%的D_(33)659m / v的压电系数。%Tb掺杂(Ba_(0.859)Ca_(0.141))(Zr_(0.106)Ti_(0.894))O_3,CaCl_2在1350℃下烧结 和残余偏振可以达到11.70μc/ cm〜2。 结果表明,优异的压电性能可能是电子行业目的的有希望的候选者。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号