The precipitation behaviors of γ″(Ni_3Nb) in four Ni-base alloys were investigated. The four alloys were forged Ni20Cr20Fe5Nb alloy, mechanically alloyed Ni20Cr20Fe5Nb alloy, IN 718 alloy and ECAPed(equal channel angular pressing) IN 718 alloy. Aging treatment was employed at either 600℃ or 720℃ for 20 hrs. The TEM observation and hardness test were performed to identify the formation of γ″. The precipitation of γ″ was noticed after aging at 600℃ for 20 hrs in the mechanically alloyed Ni20Cr20Fe5Nb alloy and ECAPed IN 718 alloy, while it was observed after aging at 720℃ for 20 hrs in the forged Ni20Cr20Fe5Nb alloy and IN 718 alloy before ECAP. It seemed that the lower aging temperature for γ″ precipitation in the mechanically alloyed Ni20Cr20Fe5Nb alloy and ECAPed IN 718 alloy than in the forged Ni20Cr20Fe5Nb alloy and IN 718 alloy before ECAP appeared to be due to the severe plastic deformation which occurred during mechanical alloying or ECAP.
机译:研究了γ”(Ni_3Nb)在四种Ni基合金中的析出行为。四种合金分别是锻造的Ni20Cr20Fe5Nb合金,机械合金化的Ni20Cr20Fe5Nb合金,IN 718合金和ECAPed(等通道角压)IN 718合金。在600℃或720℃下进行时效处理20小时。进行TEM观察和硬度测试以鉴定γ''的形成。机械合金化的Ni20Cr20Fe5Nb合金和ECAPed IN 718合金在600℃时效20小时后观察到γ″的析出,而ECAP之前的锻造Ni20Cr20Fe5Nb合金和IN 718合金在720℃时效20小时后观察到。 。看来,机械合金化的Ni20Cr20Fe5Nb合金和ECAPed IN 718合金中的γ''析出的时效温度比锻造的Ni20Cr20Fe5Nb合金和IN 718合金中的γ''析出温度低,这是由于在机械合金化或ECAP期间发生了严重的塑性变形。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号