Preparation of high sinterable Ba(Mg_(1/3)Ta_2/3))O_3 powders by hydrolysis of metal alkoxides

机译:金属醇盐的水解制备高可烧结Ba(Mg_(1/3)Ta_2 / 3))O_3粉末

获取原文
获取原文并翻译 | 示例

摘要

Ba(Mg_(1/3) STa_(2/3))O_3 {BMT} pervoskit powders have been prepared at extremely low temperatures (approx 100 deg C) by hydrolysis of Ba Mg, and Ta ethoxides. SThe alkoxides were hydrolyzed with a large amount of water (h_2O: alkoyx group molar ratio chemical bounds 10) uner refluxing to precipitate a crystalline powder with the BMT pseudo-cubic perovskite structure. The BMT powder was calcined at 1000 deg C for 3h to yeidl a sutiable powder for pressing and sintering. The calcined powder has high sinterability to provide a high-dense sintered body with the density of 94.0-98.0
机译:Ba(Mg_(1/3)STa_(2/3))O_3 {BMT} pervoskit粉末是通过Ba Mg和Ta乙醇盐的水解在极低的温度(约100摄氏度)下制备的。将醇盐用大量水水解(h_2O:alkoyx基摩尔比化学键为10),然后回流,以沉淀出具有BMT拟立方钙钛矿结构的结晶粉末。将BMT粉末在1000℃下煅烧3小时,以得到合适的粉末以进行压制和烧结。煅烧粉末具有高烧结性,从而提供密度为94.0-98.0的高密度烧结体

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号