The paper provides information about a successful evaluation and also an analysis of character of bore wear of the barrel of T-72 tank, which is still in service in number of armies throughout the world. Three types of the wear of driving parts of the barrel bore were documented. There are in original way mathematically formulated conditions of formation of a specific type of wear caused by firing the armour piercing discarding sabot 3BM-9 and 3-BM-15 projectiles in the paper.
机译:本文提供了有关成功评估的信息,还提供了T-72坦克炮管膛孔磨损特征的分析,而T-72坦克在全世界的许多军队中仍在服役。枪管孔的驱动部件的三种磨损已记录在案。最初有数学上公式化的条件来形成特定类型的磨损,这种磨损是由射击装甲的3BM-9和3-BM-15射弹击穿而造成的。

著录项

  • 来源
    《Recent researches in mechanics》|2011年|p.72-76|共5页
  • 会议地点 Corfu Island(GR);Corfu Island(GR);Corfu Island(GR);Corfu Island(GR);Corfu Island(GR);Corfu Island(GR);Corfu Island(GR);Corfu Island(GR)
  • 作者单位

    Department of Weapons and Ammunition, University of Defence, Brno, Kounicova 65, 662 10 Czech republic;

    Department of Weapons and Ammunition, University of Defence, Brno, Kounicova 65, 662 10 Czech republic;

  • 会议组织
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 机械制造工艺;
  • 关键词

    barrel bore wear; T-72 tank projectiles;

    机译:枪管内孔磨损; T-72坦克炮弹;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号