Erosion plume dynamics during pulsed laser alloying

机译:脉冲激光合金化过程中的侵蚀羽流动力学

获取原文
获取原文并翻译 | 示例

摘要

Dynamics of erosion plume during pulsed laser alloying (lambda=1.06 mum, pulse duration in millisecond range, power density 10~5-10~6 W/cm~2) of Fe with Mo, Al, Sn was analysed by means of high speed photorecording. Two qualitatively different types of plume dynamics were found: cylindrical vapour helixes and periodic pulsation. The monitoring of plume dynamics and melt ejection allows one to prevent destruction of the treated surface, to decrease the loss of doping element and to reach its uniform distribution (system: Cr shielding coating-Sn coating-Fe substrate).
机译:高速分析了Fe,Mo,Al,Sn在脉冲激光合金化过程中(λ= 1.06mum,脉冲持续时间以毫秒为单位,功率密度为10〜5-10〜6 W / cm〜2)的腐蚀羽流动力学。照相记录。发现了两种不同类型的羽流动力学:圆柱形蒸气螺旋和周期性脉动。羽流动力学和熔体喷射的监控可以防止处理表面的破坏,减少掺杂元素的损失并达到其均匀分布(系统:Cr屏蔽涂层-Sn涂层-Fe基体)。