Effect of heat input and filler metals on weld strength of gas tungsten arc welding of AISI 316 weldments

         

摘要

The present work investigates the effect of filler metals and heat input on weld bead geometry and mechanical properties of alloy316 welded by using GTAW.ER309 L,ER316 L and ERNi Cr Mo-3 filler metals,are applied to study their effect on the weldment.Weld defects are examined using radiographic testing.The mechanical properties of welds are evaluated through uniaxial testing,hardness measuring,and bending test.The mechanical properties and cooling rate decrease with increasing heat input.Tensile strength,yield stress and percentage elongation of weldments using three fillers are determined.Best results are obtained using ERNi Cr Mo-3.Besides,weld nugget area,cooling time and solidification time increases with increasing heat input.Finally,applying bending test on weld samples,cracks,tearing and surface defects are not observed.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号