摘要

采用不同方法制备了铈锆复合氧化物催化剂用于催化HCl氧化反应.自发沉积策略制备的CeO2@ZrO2催化剂中,超细CeO2纳米粒子均匀的镶嵌于非晶态ZrO2中.CeO2粒子显著的“尺寸效应”使得该催化剂具有更高的Ce3+和氧空位浓度,而较高的Ce3+和氧空位浓度使得催化剂具有优异的低温氧化还原性能和储释氧能力.催化性能测试表明,CeO2@ZrO2催化剂展现出最好的催化活性(1.90 gcl2·gcat-1·h-1),同时CeO2粒子周围非晶态的ZrO2阻碍CeO2的高温烧结,提高了该催化剂的稳定性.%Ce-Zr composite oxide catalysts were prepared by different methods for catalytic HCl oxidation.The nano-sized CeO2 particles embedded in the amorphous ZrO2 matrix fabricated by spontaneous deposition strategy.A significant "size effect" of CeO2 nanoparticles leads to considerably high concentration of Ce3+ and oxygen vacancy sites,which makes the catalyst have excellent low-temperature oxidation reduction performance and oxygen storage capacity.Catalytic performance tests indicate that the CeO2@ZrO2 catalyst shows superior activity (1.90 gC12· gcat-1· h-1) and good durability.The isolation of CeO2 nanoparticles by the amorphous ZrO2 is a key factor of durability of the catalyst.

著录项

  • 来源
    《无机化学学报》 |2017年第3期|421-428|共8页
  • 作者单位

    南京工业大学材料化学工程国家重点实验室,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学材料化学工程国家重点实验室,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学材料化学工程国家重点实验室,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学材料化学工程国家重点实验室,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学材料化学工程国家重点实验室,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学化工学院,南京210009;

    南京工业大学材料化学工程国家重点实验室,南京210009;

    南京工业大学化工学院,南京210009;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 化学动力学、催化作用;
  • 关键词

    催化氧化; 氧化铈; 氯循环; 氧空位; 尺寸效应;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号