Vanadium extraction from stone-coal was investigated by oxygen pressure acid leaching and solvent extraction.The mineralogy of the stone-coal from Tongren City of Guizhou Province,China,was investigated by various determination methods. The effects of leaching time,leaching temperature,leaching agent concentration,leaching L/S ratio,granularity of material,additive consumption were investigated based on the mineralogy.The results show that under the conditions of leaching time of 3-4 h, temperature of 150℃,sulfuric acid consumption of 25%?30%,ratio of liquid to solid of 1.2:1,the granularity less than 0.074 mm, additive consumption of 3%-5%,and oxygen pressure of 1.2 MPa,and the vanadium leaching rate can be more than 92%by the method of two-step pressurized acid leaching.The powdery V2O5 product with 99.52%in V2O5 content is obtained by the flowsheet of acid recovery,removing iron by reduction process,solvent extraction,precipitating vanadium with ammonium water,and pyrolysis from the stone-coal oxygen pressure acid-leaching solution.The total recovery efficiency of vanadium is above 85%,which is more than 20%higher than that obtained in the conventional process.Furthermore,the new process does not cause air pollution since no HCl or Cl2 is released by calcination of the raw material.
机译:通过氧压酸浸和溶剂萃取研究了从石煤中提取钒。通过多种测定方法研究了贵州铜仁市石煤的矿物学。根据矿物学研究了浸出时间,浸出温度,浸出剂浓度,浸出液L / S比,物料粒度,添加剂消耗的影响。结果表明,在浸出时间3-4h,温度150℃,硫酸消耗量为25%?30%,液固比为1.2:1,粒度小于0.074mm,添加剂消耗量为3%-5%,氧气压力为1.2MPa,钒浸出通过两步加压酸浸法可达到92%以上的收率。通过酸回收工艺流程,通过还原工艺脱铁,溶剂萃取,钒铵沉淀钒,可以得到V2O5含量为99.52%的粉状V2O5产物。水和石煤氧压酸浸液进行热解。钒的总回收率在85%以上,比常规方法高20%以上。空气污染n是因为原料煅烧不会释放HCl或Cl2。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号