The chloridizing segregation and magnetic separation of low-grade nickel laterites from Yunnan province of China was investigated.The nickel laterites were characterized by microscopic investigations,using X-ray diffractometry(XRD)and energy dispersive spectrometry(EDS)techniques.The pellets,which were prepared with magnesium chloride and coke as chloride agent and reductant respectively,were heated to a high temperature,and the pellets after cooling were crushed for magnetic separation.A series of experiments were conducted to examine the effect of chlorinating agent dosage,reductant dosage,chloridizing temperature and chloridizing time on enrichment grade of Ni and Co.The results indicate that the four factors have significant effects on the extractions of Ni and Co.The optimum conditions are as follows:the amounts of magnesium chloride and coke are 6%and 2%,respectively,chloridizing temperature is 1 253 K,and chloridizing time is 90 min.Under the conditions,extractions of Ni and Co reach 91.5%and 82.3%,respectively.
机译:研究了中国云南省低品位镍红土的氯化偏析和磁选。利用X射线衍射法(XRD)和能谱分析(EDS)技术对镍红土进行了微观研究。分别以氯化镁和焦炭作为氯化剂和还原剂制备,加热至高温,冷却后的颗粒粉碎,进行磁选。进行一系列实验,考察氯化剂用量,还原剂用量,氯化温度和氯化时间对镍和钴的富集度的影响。结果表明,这四个因素对镍和钴的萃取有显着影响。最佳条件为:氯化镁和焦炭的量分别为6%和2 %,分别为,氯化温度为1253 K,氯化时间为90 min。在此条件下,提取Ni和Co分别达到91.5%和82.3%。

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号