The specific features of current variation during different stages of the microarc oxidation process were studied on the timescale. The cathodic current was found to be closely related to the microarc discharge. The discharge was responsible for the formation of a dense coating with unique physical characteristics. A method for obtaining high-quality coating has been discussed.
机译:在时间尺度上研究了微弧氧化过程不同阶段电流变化的具体特征。发现阴极电流与微弧放电密切相关。放电负责形成具有独特物理特性的致密涂层。已经讨论了获得高质量涂层的方法。

著录项

  • 来源
    《中国物理快报:英文版》 |2001年第8期|1141-1143|共3页
  • 作者单位

    State Key Laboratory for Superhard Materials, Jilin University, Changchun 130023;

    State Key Laboratory for Superhard Materials, Jilin University, Changchun 130023;

    State Key Laboratory for Superhard Materials, Jilin University, Changchun 130023;

    State Key Laboratory for Superhard Materials, Jilin University, Changchun 130023;

  • 收录信息 中国科学引文数据库(CSCD);中国科技论文与引文数据库(CSTPCD);
  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 物理学;
  • 关键词

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号