Extraction of valuable metals from low-grade nickeliferous laterite ore by reduction roasting-ammonia leaching method

         

摘要

Nickel and cobalt were extracted from low-grade nickeliferous laterite ore using a reduction roasting-ammonia leaching method.The reduction roasting-ammonia leaching experimental tests were chiefly introduced,by which fine coal was used as a reductant.The results show that the optimum process conditions are confirmed as follows:in reduction roasting process,the mass fraction of reductant in the ore is 10%,roasting time is 120 min,roasting temperature is 1 023-1 073 K;in ammonia leaching process,the liquid-to-solid ratio is 4:1(mL/g),leaching temperature is 313 K,leaching time is 120 min,and concentration ratio of NH3 to CO2 is 90 g/L:60 g/L.Under the optimum conditions,leaching efficiencies of nickel and cobalt are 86.25% and 60.84%,respectively.Therefore,nickel and cobalt can be effectively reclaimed,and the leaching agent can be also recycled at room temperature and normal pressure.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号