Dept. of Materials Science & Engineering;
Shenyang Institute of Technologgy. Shenyang 110168;
China;
Dept. of Metal Forming;
Northeastern University;
Shenyang 110006;
China;
Institute of Metal Research;
Chinese Academy of Sciences;
Shenyang 110016;
Chinaheoretical analyses show that the variation of wall thickness is in direct proportion to outer-diameter;
inter-diameter;
and (1+R_s)~(1/2) (Rs is sectional increase ratio of tube);
the theoretical calculated results of wall thickness during tube dieless upsetting are very approximate to the experimental one. As the width of deformation field increases;
both the variation of wall thickness and the derivative of wall thickness variation to width of deformation field (to/tf) reduce.;
无模锻压; 墙体厚度; 速率场; 管道; 柔性金属制造技术;