摘要

广西河池某冶炼厂氧化酸浸—络合法浸出获得的含锑、铜浸出液中锑、铜含量分别为538. 51 mg/L、395. 91 mg/L. 对该浸出液进行水解沉淀法回收锑,沉锑残液Na2 S沉淀法回收铜的试验研究,结果表明:在搅拌强度为150 r/min、反应温度为56 ℃、反应时间为20 min、反应终了pH=3. 15条件下水解沉锑,可获得锑品位、沉淀率分别为10. 35%、98. 23%的沉锑产品;沉锑残液在Na2 S添加量为2. 5 g/L、搅拌强度为150 r/min、反应温度为50 ℃条件下反应10 min,反应完全后静置20 min进行过滤,可获得铜品位、沉淀率分别为36. 92%、98. 38%的沉铜产品. 试验结果证明分步沉淀法是回收该浸出液中锑、铜的有效方法.%There is 538. 51 mg/L Sb and 395. 91 mg/L Cu in a leachate from a smelting plant in Hechi,Guangxi Prov-ince. Antimony recovery by hydrolysis precipitation method,copper recovery by Na2 S precipitation from residual liquid from an-timony precipitation on the leachate experiment results showed that antimony hydrolysis precipitation at the stirring speed of 150 r/min,reaction at 56 ℃for 20 min,final pH=3. 15,precipitation antimony products with antimony grade and precipitation rate of 10. 35%,98. 23% is obtained. Residual liquid from antimony precipitation with Na2 S dosage of 2. 5 g/L,stirring speed of 150 r/min,reaction at 50 ℃for 10 min,stewing for 20 min and then enduring filtration,precipitation copper products with copper grade and precipitation rate of 36. 92%,98. 38% is obtained. The tests proved that fractional precipitation is a feasible method to recycle antimony,copper from the leachate.

著录项

  • 来源
    《金属矿山》 |2015年第10期|178-183|共6页
  • 作者单位

    北京科技大学土木与环境工程学院,北京100083;

    金属矿山高效开采及安全教育部重点实验室,北京100083;

    北京科技大学土木与环境工程学院,北京100083;

    金属矿山高效开采及安全教育部重点实验室,北京100083;

    北京科技大学土木与环境工程学院,北京100083;

    金属矿山高效开采及安全教育部重点实验室,北京100083;

    北京科技大学土木与环境工程学院,北京100083;

    金属矿山高效开采及安全教育部重点实验室,北京100083;

    北京科技大学土木与环境工程学院,北京100083;

    金属矿山高效开采及安全教育部重点实验室,北京100083;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 TD925.7;
  • 关键词

    浸出液; 水解沉淀回收锑; Na2; S沉淀回收铜; Sb(OH)3; CuS;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号