某钒钛磁铁矿含TFe16.43%、TiO24.70%,属表外矿.矿石组成复杂,金属矿物主要为钛铁矿、钛磁铁矿,脉石矿物主要为辉石、斜长石、角闪石和橄榄石.针对矿石性质,采用预分选-阶段磨选流程选钛,获得了TFe品位57.58%,TFe回收率60.42%的铁精矿产品;选铁尾矿采用强磁-浮选流程选钛,获得了TiO2品位46.23%,浮选作业回收率71.24%的钛精矿产品,实现了原矿中铁、钛的较好回收.%A titano-magnetite ore containing 16.43% Tfe and 4.70% TiO2,belongs to the boundary ore.The ore composition is complex,ilmentite,titano-magnetite as the main metal minerals and pyroxene,plagioclase,hornblende and olivine as the main gangue minerals.The pre-separation-stage grinding separation flowsheet was developed based on the properties of the ore and the iron concentrate with Tfe grade of 57.58% and recovery of 60.42% can be obtained.The flowsheet of high-intensity separation-flotation was adopted for the tailings to recover the ilmentite,and the qualified titanium concentrate containing 46.23% TiO2 with a recovery of 71.24% is obtained.The combined flowsheet developed to recover the ilmentite and titano-magnetite realized the comprehensive ultilization of the ore.

著录项

  • 来源
    《矿产综合利用》 |2017年第3期|67-70|共4页
  • 作者单位

    中国地质科学院矿产综合利用研究所;

    中国地质调查局金属矿产资源综合利用技术研究中心国土资源部钒钛磁铁矿综合利用重点实验室;

    四川 成都610041;

    中国地质科学院矿产综合利用研究所;

    中国地质调查局金属矿产资源综合利用技术研究中心国土资源部钒钛磁铁矿综合利用重点实验室;

    四川 成都610041;

    中国地质科学院矿产综合利用研究所;

    中国地质调查局金属矿产资源综合利用技术研究中心国土资源部钒钛磁铁矿综合利用重点实验室;

    四川 成都610041;

    中国地质科学院矿产综合利用研究所;

    中国地质调查局金属矿产资源综合利用技术研究中心国土资源部钒钛磁铁矿综合利用重点实验室;

    四川 成都610041;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 黑色金属矿选矿;
  • 关键词

    钒钛磁铁矿; 综合利用; 钛铁矿; 浮选;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号