采用响应面方法和中心复合旋转设计对低品位锰矿浸出过程建模与优化

         

摘要

采用实验设计软件对从低品位锰矿中浸出提取锰的过程进行优化.在中心复合响应面实验设计中,考察了4个主要影响浸出过程的参数,即硫酸浓度、草酸浓度、浸出时间和温度.将锰和铁的浸出率作为考察指标.采用统计分析和方差分析确定了最优条件,即最高的锰和铁浸出率、最短的浸出时间和最低的温度.结果表明,硫酸浓度是影响浸出过程的最显著的参数,在最优条件下:硫酸浓度7%,草酸浓度42.5g/L,浸出时间60 min,反应温度65℃,锰和铁的浸出率可分别达到93.44%和15.72%.%The application of leaching process to extracting Mn from a low-grade manganese ore was investigated using a software based design of experiments.Four main parameters,i.e.sulfuric acid concentration,oxalic acid concentration,time and temperature were considered in a central composite response surface design.The recoveries of Mn and Fe were selected as response of design.The optimum conditions under which the Mn and Fe recoveries were the highest and the time and temperature were the lowest were determined using statistical analysis and analysis of variance(ANOVA).The results showed that Mn and Fe recoveries were 93.44% and 15.72% under the optimum condition,respectively.Also,sulfuric acid concentration was the most effective parameter affecting the process.The amounts of sulfuric and oxalic acid were obtained to be 7% and 42.50 g/L in optimum condition and the best time and temperature were 65 min and 63 ℃.

著录项

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号