Flexural strength and microstructure of two lithium disilicate glass ceramics for CAD/CAM restoration in the dental clinic

机译:牙科诊所中用于CAD / CAM修复的两种二硅酸锂玻璃陶瓷的抗弯强度和微观结构

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

ObjectivesThere has been a growing interest in glass ceramic systems with good esthetics, high fracture resistance and bonding durability, and simplified fabrication techniques using CAD/CAM. The aim of this study is to compare flexural strength before and after heat treatment of two lithium disilicate CAD/CAM blocks, IPS e.max CAD (Ivoclar Vivadent) and Rosetta SM (Hass), and to observe their crystalline structures.
机译:目标人们对具有良好美学,高抗断裂性和粘结耐久性以及使用CAD / CAM的简化制造技术的玻璃陶瓷系统越来越感兴趣。本研究的目的是比较两种二硅酸锂CAD / CAM块IPS e.max CAD(Ivoclar Vivadent)和Rosetta SM(Hass)热处理前后的弯曲强度,并观察它们的晶体结构。