LiCoMnO_4 materials have been synthesized via a hydrothermal approach followed by a post-annealing process. Pure phase of LiCoMnO_4 is unable to form under hydrothermal conditions; however, high quality of pure LiCoMnO_4 was achieved after annealing the hydrothermal products. The concentration of LiOH and the post-annealing temperature are the crucial factors to form LiCoMnO_4. Without post-annealing process, the highest contents of LiCoMnO_4 in the hydrothermal products are less than 50% (e.g., in the presence of 1.2-1.35 M LiOH); in contrast, in the cases of 1.35-1.4 M LiOH, almost pure phase of LiCoMnO_4 has been achieved successfully after annealing the hydrothermal precursors at 750℃. The as-prepared sample in the presence of 1.35 M LiOH, after annealed at 750℃, exhibits a capacity of 91.6 mAh g~(-1).
机译:LiCoMnO_4材料已经通过水热方法合成,然后进行了后退火工艺。 LiCoMnO_4的纯相在水热条件下无法形成。然而,在对水热产物进行退火之后,获得了高质量的纯LiCoMnO_4。 LiOH的浓度和退火后的温度是形成LiCoMnO_4的关键因素。如果不进行后退火处理,则水热产物中LiCoMnO_4的最高含量小于50%(例如,在1.2-1.35 M LiOH的存在下);相反,在1.35-1.4 M LiOH的情况下,将水热前体在750℃退火后,成功地获得了几乎纯的LiCoMnO_4相。制备的样品在1.35 M LiOH存在下,在750℃退火后,具有91.6 mAh g〜(-1)的容量。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号