Development of Metakaolin as a Pozzolanic Material from Local Natural Material, Soorh

机译:亚赤素的开发作为来自局部天然材料,苏尔赫的火山醇材料

获取原文
获取原文并翻译 | 示例
           

摘要

This research aims to investigate and present the effect of extent of temperature and duration of heating on the pozzolanic properties and reactivity of the local available natural material, Soorh. The Soorh is activated by heating in a furnace chamber at temperatures 650, 700, 750 and 800 °C for 2, 3 and 6 h and at 900 and 1000 °C for 2-h duration. The energy- dispersive spectrometry and X-ray diffraction (XRD) are conducted to verify the presence of silica content and amorphous silica in developed metakaolin. The strength activity index (SAI) of developed metakaolin is determined with 20 % replacement of cement with metakaolin as per ASTM. The obtained results of SAI verdict that the optimal activation temperature is 800 °C with 2-h duration. The XRD analysis confirmed pozzolanic activity of developed metakaolin and validated the results of SAI. Moreover, it is observed that the activated metakaolin has an appreciable influence on the increase in compressive strength of the mortars.
机译:本研究旨在调查和呈现对局部可用的天然材料的波佐性能和反应性的热量和持续时间的影响。通过在温度650,700,750和800℃的炉室中加热2,3和6小时,在900和1000℃下加热到2-H持续时间,通过在炉室中加热来激活。进行能量分散光谱和X射线衍射(XRD)以验证在发育的MetaKaolin中存在二氧化硅含量和非晶二氧化硅。开发式甲霉素的强度活动指数(SAI)测定,用20%的水泥用METAKAOLIN替代水泥,根据ASTM。所获得的SAI判决结果,最佳活化温度为800℃,持续2-H℃。 XRD分析证实了开发型叶绿素的Pozzolanic活性,并验证了SAI的结果。此外,观察到活化的MetaKaolin对迫击炮的抗压强度的增加具有明显的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号