Study on the in Vitro Degradation Behavior of Commercial Zn– 4%Al–Sr Alloy for Biomedical Applications

机译:商业化生物医学应用Zn–4%Al–Sr合金的体外降解行为研究

获取原文
           

摘要

Zn and Zn-based alloys have been recognized as potential biodegradable materials, due to their proven biocompatibility and lower corrosion rates compared to Mg alloys. However, pure Zn has poor mechanical properties while Zn–4wt.% Al alloy (Zn–4Al) degrades in a nonuniform manner. In this study, Sr was used as a promising alloying element to improve the uniform corrosion properties of Zn– 4Al alloy. Microstructure and in vitro degradation behavior of Zn–4Al alloys with addition of different concentrations of Sr (0–0.15 wt%) were systematically investigated. Increasing Sr addition progressively decreased the volume fraction of primary η-Zn phase and progressively increased the (β+η) lamellar eutectic morphology. The alloy with 0.1 wt% Sr displayed the best corrosion resistance. Most importantly, the Zn–4Al–0.1Sr alloy exhibited a more uniform corrosion mode in Hanks' solution, which could reduce stress concentration and rapid reduction in the mechanical integrity.
机译:锌和锌基合金由于与镁合金相比具有良好的生物相容性和较低的腐蚀速率,因此被认为是潜在的可生物降解材料。但是,纯锌的机械性能较差,而Zn–4wt。%的铝合金(Zn–4Al)会以不均匀的方式降解。在这项研究中,Sr被用作一种有希望的合金元素,以改善Zn-4Al合金的均匀腐蚀性能。系统地研究了添加不同浓度的Sr(0-0.15 wt%)的Zn-4Al合金的显微组织和体外降解行为。增加Sr的添加量会逐渐降低初级η-Zn相的体积分数,并逐渐增加(β+η)层状共晶形态。具有0.1 wt%Sr的合金显示出最佳的耐腐蚀性。最重要的是,Zn–4Al–0.1Sr合金在汉克斯溶液中表现出更均匀的腐蚀模式,这可能会降低应力集中并迅速降低机械完整性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号