This in vitro study aimed to evaluate the effect of two different polymer-based CAD/CAM materials; resin-nano ceramic (Lava Ultimate ) and composite (CERASMART ), their different surface pre-treatments, and use of different resin cements on the μTBS of adhesively bonded CAD/CAM onlays to dentin. CAD/CAM materials were cut into slabs and divided into five groups according to the surface pre-treatments applied: Silane Primer, OptiBond XTR adhesive, Silane Primer+OptiBond XTR adhesive, Single Bond Universal (SBU), and RelyX Ceramic Primer+SBU. The LVU and CS specimens were bonded to the mid-coronal dentin of 50 non-carious human molars using NX3 resin cement with OptiBond XTR or RelyX Ultimate with SBU. μTBS was evaluated after 5,000 thermocycling and analysed with three-way-ANOVA and post-hoc Tukey’s tests (p <0.05). The μTBS was significantly influenced by the type of CAD/CAM material (p <0.0001) surface pre-treatments (p <0.05) and resin cements (p <0.05). Regardless of the pre-treatments and resin cements, bonding of the composite CAD/CAM material to dentin was higher than the resin nano-ceramic material.
机译:这项体外研究旨在评估两种不同的基于聚合物的CAD / CAM材料的效果;树脂-纳米陶瓷(Lava Ultimate)和复合材料(CERASMART),它们的不同表面预处理以及在粘结到CAD / CAM牙本质上的μTBS上使用不同的树脂胶粘剂。根据应用的表面预处理将CAD / CAM材料切成平板,分为五组:硅烷底漆,OptiBond XTR粘合剂,硅烷底漆+ OptiBond XTR粘合剂,单键通用(SBU)和RelyX陶瓷底漆+ SBU。使用带有OptiBond XTR的NX3树脂胶浆或带有SBU的RelyX Ultimate,将LVU和CS标本粘合到50个非龋齿的人类臼齿的冠状中间牙本质上。在进行5,000次热循环后,对μTBS进行了评估,并通过三向ANOVA和事后Tukey测试进行了分析( p <0.05)。 μTBS受CAD / CAM材料(> 0.0001)表面预处理(> 0.05)和树脂胶粘剂(> 0.05)的显着影响。无论采用何种预处理和树脂胶粘剂,CAD / CAM复合材料与牙本质的结合均高于树脂纳米陶瓷材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号