SFC (Sillico-Ferrite of Calcium) is a kind of simplified SFCA (Sillico-Ferrite of Calcium and Aluminum) with no Al_(2)O_(3). SFC and SFCA are believed to be the most desirable bonding phase in sinter. In order to better understand the fundamentals of the reduction of SFC, a series of experiments on the SFC reduction were carried out in the present work, including phase equilibria tested by XRD, morphology tested by SEM-EDS, and reduction pathway under the different CO/CO_(2) mixture gas at 1000°C. The experimental results indicated, (1) in the case of CO = 20% and 40%, most of Fe_(2)O_(3) in SFC was reduced to FeO. The equilibrium phases were FeO, CaO·Fe_(2)O_(3), and CaO·SiO_(2). (2) In the case of CO = 60%, CaO·Fe_(2)O_(3) was reduced to generate FeO and 2CaO·Fe_(2)O_(3). The equilibrium phases were FeO, 2CaO·Fe_(2)O_(3), and CaO·SiO_(2). (3) In the case of CO = 80% and 90%, FeO was reduced to Fe, and 2CaO·Fe_(2)O_(3) was reduced to generate Fe and CaO. The equilibrium phases were Fe, CaO, and CaO·SiO_(2). The findings from this work may provide guidelines for the improvement of sintering production and blast furnace performances.
机译:SFC(Sillico-铁素体的钙)是一种简化的SFCA(Sillico-铁素体的钙和铝),NO AL_(2)O_(3)。据信SFC和SFCA是烧结中最理想的粘合相。为了更好地理解SFC减少的基本原理,在本作工作中进行了一系列关于SFC还原的实验,包括通过XRD测试的相平衡,SEM-EDS测试的形态,不同的CO下的减少途径/ CO_(2)在1000℃下的混合物气体。所示的实验结果(1)在CO = 20%和40%的情况下,SFC中的大部分Fe_(2)O_(3)降至Feo。平衡阶段是Feo,CaO·Fe_(2)O_(3)和CaO·SiO_(2)。 (2)在CO = 60%的情况下,CaO·Fe_(2)O_(3)减少以产生Feo和2cao·fe_(2)O_(3)。平衡阶段是Feo,2caO·Fe_(2)O_(3)和CaO·SiO_(2)。 (3)在CO = 80%和90%的情况下,将Feo降至Fe,2caO·Fe_(2)O_(3)减少以产生Fe和CaO。平衡阶段是Fe,CaO和CaO·SiO_(2)。这项工作的调查结果可以为改善烧结生产和高炉表演提供指导方针。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号