Large-scale fiberform nanostructures (LFN) are formed on the tungsten (W) surface with He-W co-deposition environments. In this study, we conducted annealing experiments at 1473 - 1673 K for 30 min using an infrared heating furnace. It was found that the LFN retained their structures after annealing at 1673 K. Through detailed observations using an optical microscope, a scanning electron microscope (SEM), and a transmission electron microscope (TEM), the morphological changes are discussed in relation to the high-temperature stability.
机译:用HE-W的共沉积环境在钨(W)表面上形成大规模的纤维型纳米结构(LFN)。 在这项研究中,我们使用红外线加热炉在1473 - 1673K下进行退火实验30分钟。 发现LFN在1673K下退火后保留其结构。通过使用光学显微镜的详细观察,扫描电子显微镜(SEM)和透射电子显微镜(TEM),与高位相比讨论了形态学变化 - 温度稳定。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号