Two pass hot rolling experiments have been carried out on 3 percent Si steel rolled to total strains in the range 0.25 to 1.1 at temperatures of 850 to 1 100 deg C. Retardation of recrystallization after the second pass compared with after a single pass to the same total strain arises mainly from differences in the strain path history when only recovery takes place between passes. When partial interpass recrystallization occurs, rolling load in the second pass, recrystallization kinetics after the second pass and recrystallized grain size all follow laws of mixtures between the values for zero and full interpass recrystallization.
机译:在850至1100摄氏度的温度下,对3%的硅钢轧制到0.25至1.1的总应变进行了两遍热轧实验。当在两次通过之间仅发生恢复时,总应变主要来自应变路径历史的差异。当发生部分道间再结晶时,第二道次的轧制载荷,第二道次之后的再结晶动力学和再结晶的晶粒尺寸均遵循零值和完全道次再结晶值之间的混合规律。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号