The effect of TiB2 addition on sinterability and mechanical properties of B4C material was investigated. It was found that addition of TiB2 aids the sintering process and permits pressureless sintering at temperatures between 2050 and 2150 °C. This also alleviates grain growth during sintering. The relative density reaches 98.5% of the theoretical density by increasing the percentage of TiB2 in the composition. The mechanical properties such as hardness, fracture toughness, and bending strength were improved remarkably by addition of TiB2.
机译:研究了TiB2 对B4C材料烧结性和力学性能的影响。发现添加TiB 2有助于烧结过程,并允许在2050和2150°C之间的温度下进行无压烧结。这也减轻了烧结过程中的晶粒生长。通过增加TiB2 在组合物中的百分比,相对密度达到理论密度的98.5%。添加TiB2 可显着提高硬度,断裂韧性和弯曲强度等机械性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号