Electrical conduction in 1 mol% Sr-doped Bi4(SiO4)3 with the eulytite-type structure at elevated temperatures was investigated with conductivity measurements. Conductivity of the material under wet condition was higher than that under dry condition, and were 1.2 × 10?6 – 9.7 × 10?5 S cm?1 at 500–850 °C. From H/D isotope effects and p(O2)-dependencies of the conductivity, it was found that the Sr-doped Bi4(SiO4)3 exhibited protonic conduction at all the temperatures investigated while contribution of p-type conduction became significant with increasing p(O2) and/or temperature. Protonic and p-type conductions in the material were discussed in terms of defect equilibria.
机译:通过电导率测量研究了1 mol%的Sr掺杂Bi4 (SiO4 )3 在高温下具有真绿沸石型结构的导电性。湿态条件下的电导率高于干态条件下的电导率,在500–850°时为1.2×10?6 – 9.7×10?5 S cm?1 / sup> C。从H / D同位素效应和电导率的p(O2 )依赖性,发现掺Sr的Bi4 (SiO4 )3 在200nm处表现出质子传导。在所有温度下,随着p(O2 )和/或温度的升高,p型传导的贡献变得显着。根据缺陷平衡讨论了材料中的质子和p型传导。

著录项

  • 来源
    《Journal of Materials Science》 |2007年第16期|6566-6571|共6页
  • 作者单位

    Graduate School of Human and Environmental Studies Kyoto University Sakyo-ku Kyoto 606-8501 Japan;

    Graduate School of Human and Environmental Studies Kyoto University Sakyo-ku Kyoto 606-8501 Japan;

    Graduate School of Human and Environmental Studies Kyoto University Sakyo-ku Kyoto 606-8501 Japan;

    Graduate School of Energy Science Kyoto University Sakyo-ku Kyoto 606-8502 Japan;

    Graduate School of Science Kyoto University Sakyo-ku Kyoto 606-8502 Japan;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号