Typical α-sialon and mixed α-β sialon starting compositions were densified by either hot pressing or pressureless sintering using the oxides of Yb, Dy, Sm and Nd. The resulting materials were heat-treated at 1450 deg.C for up to 720 hours (1 month) to observe α→β sialon transformation. The results of microstructu4ral characteristics and the phase assembly showed that the high temperature stability of α-sialon phase depends on the starting composition, the type of rare earth sintering additives, the amount and viscosity of the liquid phase, and the presence or absence of β-sialon grains in the initial sintered material.
机译:通过使用Yb,Dy,Sm和Nd的氧化物进行热压或无压烧结,使典型的α-赛隆和混合的α-β赛隆起始组合物致密化。将所得材料在1450℃下热处理最多720小时(1个月),以观察α→β赛隆转变。微观结构特征和相组装的结果表明,α-赛隆相的高温稳定性取决于起始成分,稀土烧结添加剂的类型,液相的量和粘度以及β的存在与否。初始烧结材料中的-赛隆晶粒。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号