A Process for production of novel synthetic crystalline porous alumino silicate Zeolite Na-P consisting of the oxides of silicon and aluminium represented by the formula a Na_2O:Al_2O_3: b SiO_2,wherein a = 0.1-1.0 and b =2.2-5.0 has been developed from three different raw materials viz. Sodium Aluminate Liquor/ Spent Liquor/Alumina Tri-hydrate of NALCO’s Alumina Refinery, Damanjodi, Orissa . Zeolite Na-P was produced by preparing a gel by mixing Sodium Silicate, Sodium Aluminate Liquor/Spent Liquor/Alumina Tri - hydrate, autoclaving the gel at 80-150 Degree Celsius for a period of 2 hrs to 4 days under static or stirred condition, quenching the resultant crystalline material in cold water, separating the catalyst formed, washing with water, drying the solid catalyst at a temperature of 80-120 Degree Celsius for a period of 3-12 hrs to obtain the product which can be used as a builder material for detergent formulation.
机译:已开发出一种新型合成晶体多孔硅铝酸盐沸石Na-P的生产方法,该沸石由硅和铝的氧化物组成,分子式为Na_2O:Al_2O_3:b SiO_2,其中a = 0.1-1.0,b = 2.2-5.0来自三种不同的原料NALCO氧化铝精炼厂(奥里萨邦)的铝酸钠液/废液/三水合氧化铝。 Na-P沸石是通过将硅酸钠,铝酸钠液/废液/氧化铝三水合物混合制备凝胶而制成的,在静态或搅拌条件下将凝胶在80-150摄氏度下高压灭菌2小时至4天。 ,在冷水中淬灭所得结晶物质,分离形成的催化剂,用水洗涤,将固体催化剂在80-120摄氏度的温度下干燥3-12小时,以获得可以用作固体的产物。洗涤剂配方的助洗剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号