机译:氮添加量和退火温度对Ti-Nb-Zr-Ta合金超弹性性能的影响
Institute of Materials Science, University of Tsukuba, Tsukuba, Ibaraki 305-8573, Japan;
Institute of Materials Science, University of Tsukuba, Tsukuba, Ibaraki 305-8573, Japan;
Precision and Intelligence Laboratory, Tokyo Institute of Technology, Yokohama 226-8503, Japan;
School of Materials Science and Engineering & ERI, Gyeongsang National University, 900 Gozwadong, Jinju, Cyeongnam 660-701, Korea;
Institute of Materials Science, University of Tsukuba, Tsukuba, Ibaraki 305-8573, Japan,School of Materials Science and Engineering & ERI, Gyeongsang National University, 900 Gozwadong, Jinju, Cyeongnam 660-701, Korea;
shape memory alloys; superelasticity; Ti alloys; nitrogen;
机译:退火温度对Ti-Au-Cr-Zr合金组织和超弹性性能的影响
机译:添加氮的Ti-10V-2Fe-3Al合金的超弹性
机译:含氮的β钛合金的超弹性
机译:氮添加对Ti-Nb-Zr-Ta合金形状记忆性能的影响
机译:添加钼和热处理对AA3004合金高温性能的影响。
机译:Ti-6Al-4V合金不同温度退火后Ni / Cu / Ni涂层的摩擦学性能。
机译:退火温度对Ti-4Au-5Cr-8zr-8zr生物医学过度合金纹理形成的影响
机译:稀土添加剂对钛合金性能的影响。添加铒,钇和氧化钇的Ti-6al-4V的室温拉伸性能和断裂韧性。