Sintering behavior, microstructure and microwave dielectric properties of Li_(2+x)TiO_3(0≤x≤0.2) ceramics have been studied by X-ray diffraction (XRD), scan electron microscopy (SEM), Raman spectra, dilatometery and microwave resonant measurement in this research. Homogeneous non-stoichiometric composition with rock salt structure existed for Li_(2+x)TiO_3(0≤x≤0.2) ceramics. The sintering temperature was successfully reduced and highly densified sample could be obtained with appropriate excessive amount of lithium (x=0.08). A transient reactive liquid phase sintering mechanism was proposed. The preferred orientation of grain growth and micro-cracks existed in the Li_2TiO_3 (x=0) sample disappeared in the lithium excessive samples with x > 0.08. The microwave dielectric properties varied significantly with the excessive amount of lithium. Optimized microwave dielectric properties were obtained for the x = 0.08 composition: ε_r=24.6, Q×∫= 66,000 GHz, and τ_f = 22.1 ppm/℃
机译:通过X射线衍射(XRD),扫描电子显微镜(SEM),拉曼光谱,膨胀计和微波共振研究了Li_(2 + x)TiO_3(0≤x≤0.2)陶瓷的烧结行为,微观结构和微波介电性能。本研究中的测量。 Li_(2 + x)TiO_3(0≤x≤0.2)陶瓷中存在具有盐分结构的均相非化学计量组成。成功降低了烧结温度,并且可以通过添加适量过量的锂(x = 0.08)获得高致密化的样品。提出了一种瞬态反应液相烧结机理。 Li_2TiO_3(x = 0)样品中存在的晶粒长大和微裂纹的优选取向在锂过量样品中消失,x> 0.08。微波介电性能随锂的过量而显着变化。对于x = 0.08的成分,获得了优化的微波介电性能:ε_r= 24.6,Q×∫= 66,000 GHz和τ_f= 22.1 ppm /℃

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号