Synthesis of CaTiO_3:Pr persistent phosphors by a modified solid-state reaction

机译:改性固相反应合成CaTiO_3:Pr持久性磷光体

获取原文
获取原文并翻译 | 示例
           

摘要

Using tetra-n-butyl titanate and calcium nitrate as raw materials, the praseodymium-doped calcium titanates have been synthesized via a modified solid-state reaction. The decomposition process of the precursor, crystallization, and particle sizes of CaTiO_3:Pr have been investigated by using thermal analysis, powder X-ray diffraction and transmission electron microscopy (TEM). TG-DTG curves and X-ray diffraction analysis indicate that crystalline calcium titanate has been synthesized at calcining temperature of 600℃ for 2h. Photoluminescence and decay curves show that the sample obtained at the sintering temperature of 900℃ exhibited the optimal luminous property.
机译:以钛酸四正丁酯和硝酸钙为原料,通过修饰的固相反应合成了掺ody钛酸钙。通过热分析,粉末X射线衍射和透射电子显微镜(TEM)研究了CaTiO_3:Pr的前驱体的分解过程,结晶和粒径。 TG-DTG曲线和X射线衍射分析表明,在600℃的煅烧温度下2h合成了钛酸钙晶体。光致发光和衰减曲线表明,在900℃的烧结温度下获得的样品具有最佳的发光性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号