Technical Notes: Press forming analysis of aluminum auto body panel: Wrinkle behavior in 5000 and 6000 series aluminum alloy Sheet forming

机译:技术说明:铝车身板的冲压成形分析:5000和6000系列铝合金的起皱行为板材成形

获取原文
获取原文并翻译 | 示例
           

摘要

Wrinkle behavior in forming various aluminum alloys for auto body panel was analyzed, and the following results are found: Aluminum alloy generally forms more wrinkles Than steel, especially 6000 series aluminum alloy has A tendency to form more wrinkles than 5000 series. The reason for more wrinkles in 6000 series alloy is The lower break limit BHF and a drawbead restraining Force in forming conditions, and smaller n and r values in Mechanical properties. 6000 series alloy with higher yield strength forms more wrinkles, so it is important to control the yield strength.
机译:分析了在形成各种用于车身面板的铝合金中的皱纹行为,并得出以下结果:铝合金通常比钢形成更多的皱纹,尤其是6000系列铝合金比5000系列具有更多皱纹的趋势。 6000系列合金中出现更多皱纹的原因是:在成形条件下,断裂极限BHF较低,并且拉延筋抑制力较大,而机械性能中的n和r值较小。具有较高屈服强度的6000系列合金会形成更多的皱纹,因此控制屈服强度很重要。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号