Study of the Aurivillius phases Bi_4Sr_(n-3)Ti_nO_(3n+3) (n = 4, 5) synthesized by mechanochemical activation

机译:力学化学活化合成Bi_4Sr_(n-3)Ti_nO_(3n + 3)(n = 4、5)Aurivillius相的研究

获取原文
获取原文并翻译 | 示例
           

摘要

The mechanochemical activation method allows one to obtain the Aurivillius phases Bi_4SrTi_4O_(15) and Bi_4Sr_2Ti_5O_(18) with a significant decrease in the temperature of synthesis and reaction time, as compared to the solid-state method, by supplying mechanical energy to the initial reagents. The method leads to homogeneous, activated precursors, whose particle size is reduced to around 250 nm. Further thermal annealing makes crystallinity and particle size to increase. The products are characterized by Raman spectroscopy, X-ray diffraction, thermal analysis and scanning electron microscopy.
机译:通过机械化学活化方法,通过向初始试剂提供机械能,与固态方法相比,可以在合成温度和反应时间显着减少的情况下获得Aurivillius相Bi_4SrTi_4O_(15)和Bi_4Sr_2Ti_5O_(18)。 。该方法产生均质的活化前体,其粒径减小至约250 nm。进一步的热退火使结晶度和粒度增加。产品通过拉曼光谱,X射线衍射,热分析和扫描电子显微镜进行表征。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号