Studies on low pressure air plasma treatment to tasar (antheraea mylitta d.), muga (antheraea assama ww.) and eri (philosamia ricini b.)silk

机译:Studies on low pressure air plasma treatment to tasar (antheraea mylitta d.), muga (antheraea assama ww.) and eri (philosamia ricini b.)silk

获取原文
获取原文并翻译 | 示例
           

摘要

In this study, Tasar, muga and eri silk yarns were treated with low pressure air plasma. Tensile properties were evaluated in original and after plasma treatment. The tenacity of tasar, muga and eri was 2.4 g/den, 3.9 g/den and 1.6 g/den in original in comparison to 2.3 g/den, 4.0 g/den and 1.5 g/den after plasma treatment. The pair of original values and plasma treatment experimental values for elongation of tasar, muga and eri yarns are recorded as 31.9 and 30.4, 41.7 and 42.1 , and 28.5 and 24.3 , respectively. The plasma treated and controlled yarns of tasar, muga and eri with respect to wicking height was measured as 0.1 cm and 0.4 cm, 0.1 cm and 0.5 cm and 1.0 cm and 1.5 cm, respectively. Though tenacity and elongation property of tasar, muga and eri silk did not change significantly with plasma treatment, but improvement of wicking property was noticed. Surface morphology of non-mulberry silk was changed after plasma treatment.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号