AbstractThe dichroism of polypropylene film dyed with C. I. Disperse Yellow 7 was investigated at various temperatures up to 160°C. The dichroic valueDdrops as the temperature is raised. So long as the amorphous structure does not change irreversibly,Dchanges reversibly with temperature. The experimental results agree qualitatively with those obtained on poly(ethylene terephthalate) in our previous paper, although the effect of temperature on the extent of the reversible change inDis larger in PP than in PET. The plot ofDversus temperature exhibits breaks at 40°–50°C (T0), 70°–80°C (T1), and 115°–120°C (T3). These temperatures agree with the transition points of polypropylene in the literature. From the change in the intrinsic dichroismD0with temperature, it is concluded that the decrease inDat high temperatures is due to the drop ofD0caused by the disorientation of dye molecules in the amorphous region, while the amorphous polymer chain is not disoriented. Such a conclusion is supported by the fact that Δnof a heat‐set specimen is kept constant during heating,

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号