Crystallization behavior, heat resistance, and mechanical performances of PLLA/myo-inositol blends

机译:Crystallization behavior, heat resistance, and mechanical performances of PLLA/myo-inositol blends

获取原文
获取原文并翻译 | 示例
           

摘要

In this work, use of myo-inositol as a biobased nucleating agent (NA) for PLLA was researched. Effects of myo-inositol on non-isothermal and isothermal crystallization behaviors of PLLA at temperatures ranged from 85 degrees C to 130 degrees C were studied by using DSC, POM and WAXD. Isothermal crystallization kinetics results showed that the incorporation of myo-inositol enhanced significantly the crystallization rate of the PLLA samples. It was confirmed that the optimum isothermal crystallization temperature range was 100 to 110 degrees C. The above results were instructive to confirm proper heat treatment time and temperature for compression or injection molding to fabricate highly crystallized PLLA articles. The relations among heat treatment time, crystallinity, heat resistance, and mechanical performances of the neat PLLA and PLLA/1 myo-inositol specimens prepared by compression molding were investigated. Compared with the PLLA specimens, the PLLA/1 myo-inositol specimens showed a shorter heat treatment time to reach the maximum crystallinity. Vicat softening temperature, as well as tensile strength, modulus, and toughness of the PLLA/1 myo-inositol specimens was improved when crystallinity increased from 5.4 to 38.1. Considering the nontoxicity and biocompatibility of myo-inositol, PLLA/myo-inositol blends would be potential to prepare some products, which are required higher health standard and can be used in elevated temperature environments. (C) 2017 Wiley Periodicals, Inc.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号