In this paper, the fracture behavior of cracked giant magnetostrictive materials has been investigated both numerically and experimentally. Works in literature have been revisited, focusing on iron and rare-earth alloys, such as Terfenol-D. Three-point bending tests have been carried out on precracked specimens and the fracture loads have been measured in the presence and absence of a magnetic field. Recent studies on local stress fields in proximity of crack tips have shown that the Strain Energy Density (SED) can be a robust parameter in the brittle fracture assessment. Coupled-field finite element analyses have then been performed and the effect of the magnetic field on Terfenol-D fracture resistance has been discussed in terms of Energy Release Rate and averaged SED.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号