The Crack Growth Mechanism from 3-D Surface Flaw with Strain and Acoustic Emission Measurement under Axial Compression

机译:The Crack Growth Mechanism from 3-D Surface Flaw with Strain and Acoustic Emission Measurement under Axial Compression

获取原文
获取原文并翻译 | 示例
           

摘要

This paper presents the crack growth mechanism from a 3-D surface flaw on gabbro specimens using strain measurement and acoustic emission (AE) technique. Based on the results of strain and AE measurement, microcracks initiated inside the rock and extend to the surface of the specimen. With the observation from the measurements, four types of crack patterns initiate wing crack, anti-wing crack (opposite direction of wing crack), petal crack and compressive crack. The strain values of anti-wing cracks are larger 1 to 2 times than that of wing crack. The AE energy release from anti-wing crack is higher 2.5 times than that of wing crack, while the energy release form wing crack is the least but the compressive crack is the highest. Thus, the appearance of initiation and propagation of the anti-wing crack and compressive crack are very actively than that of the wing crack. The strain and AE measurement is not only to provide a clear concept on the mechanisms of crack growth form a 3-D surface flaw but also to provide useful knowledge on the AE property of the crack patterns.

著录项

获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号