Synthesis of Cu_(47)Ti_(34)Zr_(11)Ni_8 bulk metallic glass by warm extrusion of gas atomized powders

机译:

获取原文
获取原文并翻译 | 示例
           

摘要

Cu_(47)Ti_(34)Zr_(11)Ni_8 amorphous gas atomized powders were consolidated by warm extrusion. After consolidation near 723 K using an extrusion ratio of 5, the material retains between 88 percent and 98 percent of the amorphous structure found in the gas atomized powder. The onsets of the glass transition and crystallization temperatures of this extruded material are observed respectively at slightly higher and lower temperatures than those of the starting powders. These temperature shifts are attributed to a composition change in the remaining amorphous phase during partial devitrification throughout the extrusion process. Powders extruded at the same temperature, but using higher extrusion ratios of 9 and 13, exhibit substantial devitrification during the consolidation process yet still deform homogeneously.

著录项

相似文献

  • 外文文献
  • 中文文献
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号