FRICTION AND WEAR OF TITANIUM ALLOYS AND COPPER ALLOYS SLIDING AGAINST TITANIUM - 6-PERCENT -ALUMINUM - 4-PERCENT-VANADIUM ALLOY IN ADR AT 430° C

机译:钛合金和铜合金在430°C下对aDR中的6% - 4% - 4% - 钒合金滑动摩擦磨损

获取原文

摘要

Experiments were conducted to determine the friction and wear characteristics of aluminum bronzes and copper-tin, titanium-tin, and copper-silver alloys sliding against a titanium -6-percent-aluminum - 4-percent-vanadium alloy (Ti-6Al-4V). Hemispherically tipped riders of aluminum bronze and the titanium and copper alloys were run against Ti-6A1-4V disks in air at 430°C. The sliding velocity was 13 cm/sec, and the load was 250 g. Results revealed that high-tin-content titanium and copper alloys underwent significantly less wear and galling than commonly used aluminum bronzes. Also friction force was less erratic than with the aluminum bronzes.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号