The invention relates to a heat treatment of a chromium steel (4), in particular a 9% -10% chromium steel, which is used at 673K to 823K, in which oxidation is carried out beforehand in an oven, preferably in air, at which the temperature of the preoxidation is carried out is at least 20K, in particular at least 30K higher than in the area of use, preferably greater than or equal to 873K, as a result of which a pure chromium oxide layer (20) is formed.
机译:本发明涉及铬钢(4),特别是9%-10%铬钢的热处理,其在673K至823K下使用,其中氧化是预先在烘箱中,优选在空气中,在进行预氧化的温度至少比使用区域高20K,特别是至少高30K,优选大于或等于873K,由此形成纯的氧化铬层(20) 。