nanoadsorbent based on hydrated oxides of aluminium, iron and manganese removal from water arsenitanů and arseničnanů contains amorphous hydrated oxides respectively as ternary aluminium, iron,manganese in the molar ratio 0.5: 4.5: 1.5 to 3: 4.5: 1,5. the concentration of oxides of at nanoadsorbentu is up to 60% hmotn., a particle size of 10 to 100 nm, the specific surface area of 50 to 100 m2 / g.production method nanoadsorbentu lies in the fact that the solutions of salts of aluminium, iron and manganese are mixed in the molar ratio of al: fe: mn = 0.5: 4.5: 1.5 to 3: 4.5: 1.5, the addition of naoh to adjust the ph to 9.5 and 10.the mixture is allowed to age for a period of 10 to 14 hours, the solid phase is separated and dried at a temperature of 200 to 250 degrees celsius for a period of 11 to 14 hours. nanoadsorbent may be mixed with sodium na2sio3 at 25 to 35% by weight.and granulovat.
机译:基于从水中除去铝,铁和锰的水合氧化物的纳米吸附剂arsenitanů和arseničnanů分别含有非晶态水合氧化物,分别为三元铝,铁,锰,摩尔比为0.5:4.5:1.5至3:3:4.5:1,5。纳米吸附剂的氧化物浓度最高为60%hmotn。,粒径为10至100 nm,比表面积为50至100 m2 / g。生产方法纳米吸附剂的事实在于铝,铁和锰以Al:Fe:mn = 0.5:4.5:1.5至3:3:4.5:1.5的摩尔比混合,添加Naoh将pH值调节至9.5和10。在10至14小时的时间内,分离固相并在200至250摄氏度的温度下干燥11至14小时。可以将纳米吸附剂与重量百分比为25%至35%的Na2S103钠和Granulovat混合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号