The fatigue strength of a lap-welded joint, wherein an overlapping portion of a first steel material and an overlapping portion of a second steel material overlap with each other, and an edge portion of the first steel material is welded to a front face of the second steel material with a weld zone extending along the edge portion, is improved. First, when a direction perpendicular to an extending direction X of the weld zone and parallel to a front face of the second steel material is defined as a reference direction Y, the lap-welded joint is restrained from moving in the reference direction Y, and the first steel material and the second steel material are restrained from moving in their sheet-thickness directions. In this state, a portion of the second steel material is heated such that a melted portion is formed in the portion of the second steel material.
机译:搭接焊接接头的疲劳强度,其中第一钢材的重叠部分和第二钢材的重叠部分彼此重叠,并且第一钢材的边缘部分焊接到焊接的前表面。改进了具有沿边缘部分延伸的焊接区的第二钢材。首先,当将垂直于焊接区域的延伸方向X并且平行于第二钢材的正面的方向定义为基准方向Y时,搭接接头被限制在基准方向Y上移动,并且限制了第一钢材和第二钢材在其板厚方向上的移动。在这种状态下,第二钢材的一部分被加热,使得在第二钢材的一部分中形成熔融部分。

著录项

  • 公开/公告号US2019291216A1

    专利类型

  • 公开/公告日2019-09-26

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL &SUMITOMO METAL CORPORATION;

    申请/专利号US201716071158

  • 发明设计人 SHOTA KIKUCHI;MANABU FUKUMOTO;

    申请日2017-01-27

  • 分类号B23K31/02;B23K9/02;B23K26/21;B23K15;

  • 国家 US

  • 入库时间 2022-08-21 12:11:11

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号