PROBLEM TO BE SOLVED: To provide a manufacturing method of a mixed solution of NiSOand CoSOlow in chlorine concentration by adding sulfuric acid to a mixture containing at least Cl, Ni(OH)and Co(OH)and dissolving a solid component in the slurry, and removing contained chlorine constituent without specific cost increase and efficiency reduction.SOLUTION: There is provided a manufacturing method of a low chlorine concentration mixed solution of NiSOand CoSOfor obtaining a mixed solution of NiSOand CoSOlow in chlorine concentration by holding a temperature of a dissolution liquid for dissolving a solid component of the slurry at 60°C or higher, which is manufactured by adding a slurry making solution to a mixture containing at least 5 to 10 wt.% of Cl, 35 to 60 wt.% of Ni and 1 to 10 wt.% of Co to form concentration adjusted slurry having slurry concentration of 360 g/L or less and then adding sulfuric acid to the concentration adjusted slurry, and controlling pH of the dissolution liquid at 2.0 or less and dissolving the solid component of the slurry to remove Cl contained in the slurry.SELECTED DRAWING: Figure 2
机译:要解决的问题:提供一种向氯浓度低的NiSO和CoSO混合溶液的制造方法,方法是向至少包含Cl,Ni(OH)和Co(OH)的混合物中添加硫酸,并将固体成分溶解在浆料中,解决方案:提供了一种低浓度的NiSO和CoSO的混合溶液的制造方法,用于通过保持溶解液的温度来获得低浓度的NiSO和CoSO的混合溶液。在60°C或更高温度下溶解浆料的固体成分的方法,该方法是通过将浆料制备溶液添加到包含至少5至10重量%的Cl,35至60重量%的Ni和1至10的混合物中来制造的Co的重量%,以形成浓度为360g / L以下的浓度调节浆料,然后向该浓度调节浆料中添加硫酸,并控制溶解液的pH。在2.0或更低的浓度下溶解浆液中的固体成分以除去浆液中所含的Cl。图2

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号