首页> 外国专利> Low carbon neutralization-inhibiting mortar composition and low carbon neutralization-inhibiting mortar cured product

Low carbon neutralization-inhibiting mortar composition and low carbon neutralization-inhibiting mortar cured product

机译:低碳中和抑制砂浆组合物和低碳中和抑制砂浆固化产品

摘要

PROBLEM TO BE SOLVED: To provide a low-carbon neutralization-suppression mortar composition that suppresses neutralization as well as is excellent in compressive strength.SOLUTION: Provided is a low-carbon neutralization-suppression mortar composition comprising inorganic fine powder, gypsum, fine aggregate and kneading water and in which: the inorganic fine powder is composed of cement and blast furnace slag fine powder and the mass ratio of cement and blast furnace slag fine powder (cement: blast furnace slag) is from 10:90 to 30:70; the amount of gypsum is 6 to 10 pts.mass with respect to 100 pts.mass of the inorganic fine powder; and the kneading water has a pH of 10 to 14 and a Ca ion concentration of 100 to 5000 mg/L. The low-carbon neutralization-suppression mortar composition in which the kneading water has a Na ion concentration of 10 to 500 mg/L and a Ka ion concentration of 10 to 500 mg/L, and furthermore a SOion concentration of 10 to 5000 mg/L and a Cl ion concentration of 1 to 100 mg/L.SELECTED DRAWING: None
机译:解决的问题:提供一种抑制中和并具有优异的抗压强度的低碳中和抑制砂浆组合物。解决方案:提供一种包含无机细粉,石膏,细骨料的低碳中和抑制砂浆组合物。所述的无机细粉由水泥和高炉矿渣细粉组成,水泥与高炉矿渣细粉的质量比(水泥:高炉矿渣)为10:90至30:70。相对于无机细粉100质量%,石膏的量为6〜10质量%。混炼水的pH为10〜14,Ca离子浓度为100〜5000mg / L。混炼水的Na离子浓度为10〜500mg / L,Ka离子浓度为10〜500mg / L,SO离子浓度为10〜5000mg / L的低碳中和抑制砂浆组合物。 L和Cl离子浓度为1至100 mg / L。

著录项

  • 公开/公告号JP6582599B2

    专利类型

  • 公开/公告日2019-10-02

    原文格式PDF

  • 申请/专利权人 宇部興産株式会社;

    申请/专利号JP20150124605

  • 申请日2015-06-22

  • 分类号C04B28/08;C04B18/14;C04B22/14;C04B22/06;C04B40/02;B28C7;C04B111/22;

  • 国家 JP