首页> 外国专利> ASPHALT MIXTURE, METHOD OF MANUFACTURING ASPHALT MIXTURE, ASPHALT PAVEMENT METHOD, AND ASPHALT PAVEMENT BODY

ASPHALT MIXTURE, METHOD OF MANUFACTURING ASPHALT MIXTURE, ASPHALT PAVEMENT METHOD, AND ASPHALT PAVEMENT BODY

机译:沥青混合物,制造沥青混合物的方法,沥青铺面方法和沥青铺面体

摘要

To provide an asphalt mixture improving various properties and having general usefulness, a method of manufacturing the asphalt mixture, an asphalt pavement method, and an asphalt pavement body.SOLUTION: An asphalt mixture comprises an aggregate, asphalt, and an additive agent. The asphalt has penetration of 40 to 100. The additive agent consists of a terpene resin or petroleum pitch, and added at a weight ratio of 1.0 to 15.0% based on the total amount of asphalt and the additive agent. The total amount of asphalt and the additive weight is added at a weight ratio of 4.0 to 6.5% based on the asphalt mixture.SELECTED DRAWING: None
机译:为了提供改善各种性能并具有通用性的沥青混合物,该沥青混合物的制造方法,沥青路面方法和沥青路面体。解决方案:沥青混合物包括骨料,沥青和添加剂。沥青的渗透率为40到100。添加剂由萜烯树脂或石油沥青组成,并且以沥青和添加剂的总量为基准,以1.0到15.0%的重量比添加。沥青的总量和添加剂的重量以沥青混合物的重量比为4.0%至6.5%添加。

著录项

  • 公开/公告号JP2019157427A

    专利类型

  • 公开/公告日2019-09-19

    原文格式PDF

  • 申请/专利权人 NIPPO CORP;

    申请/专利号JP20180042827

  • 发明设计人 SHIRAI YU;WATANABE SHINICHI;

    申请日2018-03-09

  • 分类号E01C7/22;E01C7/26;

  • 国家 JP