首页> 外国专利> METHOD AND APPARATUS FOR PRODUCING DIRECT REDUCED IRON UTILIZING A CATALYTICAL PRETREATMENT OF HYDROCARBONS AS A SOURCE OF REDUCING GAS

METHOD AND APPARATUS FOR PRODUCING DIRECT REDUCED IRON UTILIZING A CATALYTICAL PRETREATMENT OF HYDROCARBONS AS A SOURCE OF REDUCING GAS

机译:利用碳的催化预处理直接还原铁生产还原铁的方法和装置

摘要

A method and apparatus for producing direct reduced iron, said method comprising producing direct reduced iron using a pre-treated make-up gas as a reducing agent in a direct reduced iron reactor (10), and wherein producing direct reduced iron is carried-out using a zero-reformer process in which catalytic reformation of the pre-treated make-up gas is carried-out "in situ" within the direct reduced iron reactor (10) such that the pre-treated make-up gas is subjected to no further catalytic reaction besides the catalytic reactions that occur inside said direct reduced iron reactor (10),characterized in thatsaid method comprises: - pre-treating a stream of said make-up gas containing heavy hydrocarbons by subjecting the stream of make-up gas to a low temperature adiabatic reforming at a temperature comprised between 300°C and 600°C, prior to using said stream of make-up gas as a reducing agent for producing direct reduced iron; - subjecting said pre-treated stream of make-up gas to adjusting humidity content of said stream of make-up gas after said low temperature adiabatic reforming by bypassing said stream of make-up gas to selectively split said stream into a first part (128) of said stream of make-up gas and a second part (130) of said stream of make-up gas and subjecting said first part (128) to a water separation and then mixing said first part (128) to said second part (130) to obtain a reducing stream (146) to be sent to direct reduced iron production.
机译:一种生产直接还原铁的方法和设备,所述方法包括在直接还原铁反应器(10)中使用预处理的补充气体作为还原剂生产直接还原铁,并且其中进行直接还原铁的生产使用零重整工艺,其中在直接还原铁反应器(10)内“原位”进行预处理的补充气体的催化重整,以使预处理的补充气体不经历除了在所述直接还原铁反应器(10)内发生的催化反应之外,进一步的催化反应的特征在于,所述方法包括:-通过使补充气流经受如下处理,对所述包含重烃的补充气流进行预处理。在使用所述补充气流作为还原剂以生产直接还原铁之前,在300℃至600℃之间的温度下进行低温绝热重整; -在所述低温绝热重整之后,通过使所述补充气体流经过所述补​​充气体流以选择性地将所述补充气体流分成第一部分,来使所述补充气体预处理流调整所述补充气体流的湿度。 )补充气物流和补充气物流的第二部分(130),然后对第一部分(128)进行水分离,然后将第一部分(128)与第二部分进行混合(130) 130)获得还原流(146),该还原流被送往直接还原铁的生产。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号