A method for producing calcium sulfoaluminate clinker comprising 10-100% by weight of C4A3-xFx $, varying x from 0 to 2, 0-70% by weight of C2S, 0-30% by weight of aluminates , 0-30% by weight of ferrites, 0-30% by weight of ternesite, 0-30% by weight of calcium sulfate and up to 20% by weight of minor phases, all with respect to the total weight of the clinker, comprising the following steps - providing a crude comprising at least sources of CaO, Al2O3, SO3 - agglomerating the crude in an oven at a temperature ranging from 1100 to 1350 ° C to provide a clinker - cooling the clinker, in which A flux / mineralizer comprising at least one compound containing a glass or copper powder and a glass powder is added to the crude before or during agglomeration.
机译:一种生产硫铝酸钙熟料的方法,其包含10-100重量%的C4A3-xFx $,x在0至2之间变化,0-70重量%的C2S,0-30重量%的铝酸盐,0-30重量%。相对于熟料的总重量,铁素体的重量,0-30%的菱锰矿,0-30%的硫酸钙和最多20%的次生相,包括以下步骤-提供至少包含CaO,Al2O3,SO3来源的原油-在烤箱中将其在1100至1350°C的温度范围内结块以提供熟料-冷却熟料,其中助熔剂/矿化剂包含至少一种含在团聚之前或过程中,将玻璃粉或铜粉和玻璃粉添加到原油中。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号